| SAE |
SAE AMS6305 |
Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing, and Forging Stock, 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C), Vacuum Arc Remelted |
|
| SAE |
SAE AMS5931 |
Steel, Wear, Galling, and Corrosion-Resistant Bars, Wire, Forgings, Extrusions, Mechanical Tubing, Rings, and Stock for Forgings, Rings, and Extruding, 5.0Mn - 3.5Si - 16.5Cr - 5.0Ni - 0.14N, Solution Heat Treated |
|
| SAE |
SAE AMS5664 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1950 °F (1066 °C) Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5661 |
Nickel-Iron Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging or Flash-Welded Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe (Alloy 901) Consumable Electrode Remelted or Vacuum Induction Melted Solution Heat Treated, Stabilized, and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5708 |
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Rings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated_x000D_
|
|
| SAE |
SAE AMS6304 |
Low-Alloy Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing, and Forging Stock 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) |
|
| SAE |
SAE AMS5955 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Forging Stock, 10Cr - 12Ni - 2Mo - 1.45Al - 1.15Ti, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated, Precipitation Hardenable_x000D_
|
|
| SAE |
SAE AMS5768 |
Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Rings and Stock for Forgings, Rings and Heading, 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0Cb - 0.15N - 31Fe, Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS6302 |
Low-Alloy Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing and Forging Stock, 0.65Si - 1.25Cr - 0.50Mo - 0.25V (0.28 - 0.33C) |
|
| SAE |
SAE AMS5670 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings, and Stock for Rings, Forgings, and Heading, 72Ni - 15.5Cr - 0.95Cb (Nb) - 2.5Ti - 0.70Al - 7.0Fe (X750), 1800 °F (982 °C) Solution Heat-Treated, Precipitation-Hardenable |
|
| SAE |
SAE AMS5749 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Forging Stock and Mechanical Tubing, 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C), Premium Quality for Bearing Applications, Double Vacuum Melted |
|
| SAE |
SAE AMS5935 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings and Forging Stock, 12Cr - 10Ni - 2Mo - 0.9Al - 0.3Ti, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5663 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution and Precipitation Heat Treated_x000D_
_x000D_
|
|
| SAE |
SAE AMS5620 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Forging Stock, 13Cr (0.30 - 0.40C) (420F, 420FSe), Free-Machining Grade, Annealed |
|
| SAE |
SAE AMS5662 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50AI - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable |
|
| SAE |
SAE AMS5654 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Forging Stock, 18Cr - 11Ni - 0.60Cb (Nb) (347), Premium Aircraft Quality, Consumable Electrode Melted, Solution Heat Treated |
|
| SAE |
SAE AMS7235 |
Rivets, Steel, Corrosion and Heat Resistant 15Cr 25.5Ni 1.2Mo 2.1Ti 0.006B 0.30V 1650°F (900°C) Solution Heat Treated and Partially Precipitation Heat Treated |
|
| SAE |
SAE AMS5653 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 17Cr - 12Ni - 2.5Mo (0.030 Max C) (316L), Solution Heat Treated |
|
| SAE |
SAE AMS5652 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 25Cr - 20Ni - 2.0Si (314) Solution Heat Treated_x000D_
_x000D_
|
|
| SAE |
SAE AMS5650 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 23Cr - 13.5Ni (309S), Solution Heat Treated |
|
| SAE |
SAE AMS5651 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 25Cr - 20Ni (310), Solution Heat Treated |
|
| SAE |
SAE AMS5639 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging and Ring Stock, 19Cr - 10Ni, Solution Heat Treated |
|
| SAE |
SAE AMS5659 |
Steel, Corrosion Resistant, Bars, Wire, Forgings, Rings, and Extrusions, 15Cr - 4.5Ni - 0.30Cb (Nb) - 3.5Cu, Consumable Electrode Remelted, Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5668 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al (X750) 2100 °F (1149 °C) Solution and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5648 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings and Rings, 17Cr - 12Ni - 2.5Mo (316), Solution Heat Treated |
|