1.1 This test method covers the measurement of tensile strength (breaking strength) and stretch properties (elongation and "F" value) for pressure-sensitive tapes. It includes procedures for machine direction cross-direction tests and tests for tapes with low and high stretch and reinforced backings. It also includes a procedure for obtaining stretch force ("F" value) in conjunction with a determination of tensile strength. These procedures employ a constant-rate-of-extension (CRE)-type testing machine. They apply to the principle of stretching the specimen at a fixed strain rate of 25 mm per 25 mm [1 in. per inch] of specimen length per minute with the exception of the procedure for reinforced tapes.

1.2 The values stated in either SI or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system must be used independently, without combining values in any way.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


SDO ASTM: ASTM International
Document Number D3759
Publication Date April 1, 2004
Language en - English
Page Count 6
Revision Level 04
Supercedes
Committee D10.14
Publish Date Document Id Type View
Oct. 1, 2005 D3759_D3759M-05 Revision
April 1, 2004 D3759_D3759M-04 Revision
Jan. 1, 1996 D3759_D3759M-96E01 Revision
Aug. 1, 2019 D3759_D3759M-05R19 Reaffirmation
Aug. 1, 2011 D3759_D3759M-05R11 Reaffirmation